Width:500mm-1500mm thickness:10um-300um length: customized
Beer, beverage special shrink film is a kind of PE heat shrinkable film, its characteristic is suitable for high speed automatic production, good sealing, good shrinkage, the intensity is high, the handling process not loose package, not variant, especially suitable for packing.
Specification:
Width | 350mm-750mm | |
Thickness | 60um-150um | |
Tear | TD≥55kN/m | MD≥55kN/m |
Shrinkage | TD 10%-25% | MD 60%-75% |
Tensile strength | TD≥20Mpa | MD≥20MPa |
Shrinking temperature | 180ºC-240ºC | |
Density | 0.95g/cm3 | |
Core | 76mm |


WARM PROMPT
The heat sealing temperature directly affects the heat sealing strength of the heat shrinkable film. In the process of packaging or bag making, if the heat sealing temperature is not set properly or adjusted improperly, the following two situations will occur.
1. When the thermal seal temperature is too high, exceeding the thermal shrinkage temperature of the materials on the heat-shrinkable film surface, the film body will shrink and deform, leading to shrinkage film and thermal seal adhesion occurs between the knives and the hot sealing edge material melts and extrudes, causing root cutting.
2. When the heat sealing temperature is too low, there will be bad heat sealing.
 PVC PE Shrink Protective Wrapping Film for Group Boundling
Width:500mm-1500mm thickness:10um-300um length: customized
Beer, beverage special shrink film is a kind of PE heat shrinkable film, its characteristic is suitable for high speed automatic production, good sealing, good shrinkage, the intensity is high, the handling process not loose package, not variant, especially suitable for packing.
Specification:
Width | 350mm-750mm | |
Thickness | 60um-150um | |
Tear | TD≥55kN/m | MD≥55kN/m |
Shrinkage | TD 10%-25% | MD 60%-75% |
Tensile strength | TD≥20Mpa | MD≥20MPa |
Shrinking temperature | 180ºC-240ºC | |
Density | 0.95g/cm3 | |
Core | 76mm |


WARM PROMPT
The heat sealing temperature directly affects the heat sealing strength of the heat shrinkable film. In the process of packaging or bag making, if the heat sealing temperature is not set properly or adjusted improperly, the following two situations will occur.
1. When the thermal seal temperature is too high, exceeding the thermal shrinkage temperature of the materials on the heat-shrinkable film surface, the film body will shrink and deform, leading to shrinkage film and thermal seal adhesion occurs between the knives and the hot sealing edge material melts and extrudes, causing root cutting.
2. When the heat sealing temperature is too low, there will be bad heat sealing.
Â
We are established in 2010 which is a professional HP Laserjet Printer Parts and Samsung Printer Parts.After few years development,we already have a sales department,technical and research department and production department.Our best quality products are popular in Asia,Equrope,American etc. We always insist that introduce our products into more people over the world.
Our products including,
1, Hp Printer Parts,such as Fuser Assembly ,Maintenance Kits, Formatter Board ,fuser film sleeve, pick up roller..etc
2,Samsung printer parts,such asfuser film sleeve, pick up roller, Seperation Pad , bushing etc.
Most of Samsung printer parts model are available .favorable price if large quantity.Welcome your inquiry!
Samsung Printer Part,Samsung Printer Spare Parts,Samsung Printer Parts ,Samsung Laser Printer Parts
Dunhua Office Equipment Co., Ltd. , http://www.dunhuaparts.cn